you can just cut it into small pieces, then you can do the side view under sem. On 5/24/05, csh@u.washington.eduwrote: > I have a grating sample on AZ 1512 with Si <100> as substrate. > The period is supposed to be about 0.24um. > I am wondering how to take SEM of the cross section of the grating?