Shay Kaplan
2005-06-01
It's better to freeze the samples in liquid nitrogen before cleaving -
otherwise the resist will smear. Even better to cover it with acrylic first
shay

-----Original Message-----
From: Duan
Subject: Re: [mems-talk] How to take a cross section SEM pictures?

you can just cut it into small pieces, then you can do the side view under
sem.