hi, i tried to deposit Au on glass slide using eavpporation deposition method. i deposited a 5 nm chromiun layer before depositing Au and then deposited 180nm Au layer. photoresist was used as a sacrifial layer. the Au layer (along with the desired features) came out instantly when i dipped the slide in acetone but the photoresist was still there on the slide. could someone tell me a reson for this? -- RUPESH SAWANT