Shay, the only way that the world knows how to electroplate aluminum is from
a bath of molten cryolite at a red heat.  If we have a new way to do it then
by all means lets get out of the micro world and start plating aluminum.

Gary

-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org]On Behalf Of shay kaplan
Sent: Tuesday, January 22, 2008 5:39 AM
To: 'General MEMS discussion'
Subject: RE: [mems-talk] High Thickness of Aluminum on Silicon


Do you have a recipe for electroplating aluminum? Can you share it?