Not sure what you mean. Sputtered Aluminum should be a mirror like surface because it is highly reflective for all visible wavelengths. If you are not getting a good film I would start by checking the substrate quality first. On Mon, May 19, 2008 at 10:40 AM, Brent Garberwrote: > Nataraj, > > You will need to provide a little more information as how you are depositing > the aluminum for anyone to help you. > > If you are using DC sputtering, I have found the faster the rate the better. > > Brent