Hi all--

I am wondering if anyone knows how I can deposit a 2mm (yes, 2,00um) layer
of SU-8 and pattern it.

Thanks,

Aimi Ahmad-Shukri
Dept of Mechanical Engineering
University of Washington
aimisas@u.washington.edu
cell: (206) 930-8186
lab: (206) 221-5340