You could always deposit and pattern several layers of whatever max thickness you can achieve (e.g. 4 layers of 500um thick using SU-8 2150). On Wed, Nov 26, 2008 at 2:31 PM, A. AhmadShukriwrote: > Hi all-- > > I am wondering if anyone knows how I can deposit a 2mm (yes, 2,00um) layer > of SU-8 and pattern it. > > Thanks, > > Aimi Ahmad-Shukri