Hi all!

Happy New Year, first of all!

My question is, did anybody try to electroplate gold onto Al surface.
We have tried that at our facility recently. After 15 min. absolutely
nothing happened. No gold at all.

We shall be thankful for any suggestions.

Regards,

--