I would try to deposit first a thin layer of Ti or TiN, then adhesion
should not be an issue..


On Tue, Jan 27, 2009 at 8:21 PM, Wilson, Thomas  wrote:
> Jordi,
>
> Any comment about the adhesion of gold to bare aluminum? I've read somewhere
it's pretty awful.
>