An inert gas plasma will increase the surface area giving better contact. Bill Moffat -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Javier Crespo Sent: Thursday, March 26, 2009 2:05 AM To: mems-talk@memsnet.org Subject: [mems-talk] Ti-Si Ohmic contact... Hello, Does anyone know how could I improve the ohmic contact of the sputtered Ti layer with silicon? I know that there are some differences if the Silicon is N or P-type, but in both cases I can't have a good contact. Should I use TiW in case of Ti?