I think it is not good for me because SU-8 is an epoxy-based photoresist and I need to preserve it. Emanuele 2009/11/18 Mikael Evander: > I've used a negative resist stripped called microstrip. When heated to > around 50 C it removes silicone, epoxy and god knows what. > > /Mikael