Hi all,

i need to realize silicon memabranes of thickness 29um. I can not start
from SOI wafers, cos the membrane will remain under stress state due to
the oxide in the frame.

I plan to realize the job by KOH etching, but how to precisely control the
membrane thickness ? Is there any suggestion ?

Thanks,
Andrea