Hi, All I need to deposit (e-beam evaporation) Aluminum on SU-8 2002 (developed), and there are subsequent patterning steps for aluminum. Is there anything I need to watch out? Is there any tricks to improve adhesion? Any advice would be greatly appreciated! Thanks! Sheng