Dear everyone,

I am using SU-8 2075 in photolithography. I want to get a thin film after spin
coating so i intend to use IPA to dilute su-8, but it does not work. Has anybody
encountered this problem?  How do you dilute the su-8?

Any suggestion will be highly appreciated.

Thanks in advance.
Regards