You can use PGMEA to dilute SU-8

Regards,

Jin



-----Original Message-----
From: 첸로 [mailto:baifenzhi3@126.com]
Sent: 20 April 2011 12:10
To: mems-talk
Subject: [mems-talk] dilute SU-8 2075


Dear everyone,

I am using SU-8 2075 in photolithography. I want to get a thin film after spin
coating so i intend to use IPA to dilute su-8, but it does not work. Has anybody
encountered this problem?  How do you dilute the su-8?

Any suggestion will be highly appreciated.