Hi All, Could anybody please suggest a negative tone resist that is suitable for lift-off and is stable up to 250 ° C. I want to achieve a thickness of at least 10 micron. Thanks -- Majid Beidaghi PhD Candidate Department of Mechanical and Materials Engineering Florida International University