durusmail: mems-talk: Dry etch 50nm Au film, possible?
Dry etch 50nm Au film, possible?
2011-08-11
2011-08-11
2011-08-11
2011-08-11
2011-08-11
2011-08-14
2011-08-11
2011-08-11
2011-08-14
Dry etch 50nm Au film, possible?
Shay
2011-08-11
OXIDE rie will do it

Shay

-----Original Message-----
From: mems-talk-bounces+shay=mizur.com@memsnet.org
[mailto:mems-talk-bounces+shay=mizur.com@memsnet.org] On Behalf Of Xiaohui
Lin
Sent: Thursday, August 11, 2011 2:08 AM
To: General MEMS discussion
Subject: [mems-talk] Dry etch 50nm Au film, possible?

Hi all: Is it possible to use any dry etch receipt to etch Cr/Au film
(50nm)?

The mask of etching is Ni.
reply