Hello,

I'm doing single layer SU8 2005, thickness ~6-7um. I use 60mJ/cm^-2 on sputtered
gold surface. But somehow sometimes I notice that the edges of my pattern
darkens, I suspect it's due to overexposed. But 60mJ is quite a low dose
compared to the recommended one. I would appreciate any comments given. Thank
you.

Best Regards,
Jocelyn

Sent from my iPhone