We use TOK NMD-W developer. It can be used with i-line or DUV. It is .24N.

Robert

-----Original Message-----
From: mems-talk-bounces+r-black1=ti.com@memsnet.org [mailto:mems-talk-
bounces+r-black1=ti.com@memsnet.org] On Behalf Of Jocelyn Ng
Sent: Friday, June 06, 2014 11:40 PM
To: General MEMS discussion
Subject: [mems-talk] MF CD-26 Developer

Hello,

I'm looking for replacement to the CD-26 developer. It's a TMAH based developer.
Is there any suggestion out there for the replacement developer?

Any comments and suggestions is welcomed.

Thanks lot.

Best Regards,
Jocelyn

Sent from my iPhone
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply