Can you see the place of exposed pattern after soft-bake? On 07.07.2014. 20:25, Dimitar Dimitrov wrote: > Hello, > > I am graduate student in Brooklyn College and I am trying to reinvent the whole MEMS procedure as I do not have any professional help. My science adviser is from another field. > > I am having difficulties with the developing of SU-8 2025. Here is what I am doing: > > I am spin - coating 4 inch Si or Pyrex wafer to 50 - 60 um thin film > Pre - baking at 96 degrees for 15 min > Sometimes instead I am putting the wafer in the vacuum chamber of my UV imprinter. The vacuum is taking away the solvent and clear most of the bubbles. > UV exposure with a hand made Imprinter: Xenon lamp 22kV at 10 microsec. pulses. Three 30 seconds exposures with couple of seconds pause. > UV lamp creates heat so the wafer is let for 2 - 3 min to relax. > Post bake of 15 min at 95 degrees. > > Developing by tenderly shaking the wafer in a vessel with Propylene glycol monomethyl ether forever. > > The result is that I clearly can see my pattern as exposed SU-8 is yelowish but the unexposed parts are not removed and form thin film with the exposed part. > Less exposure leads to removing all of the polymer. > (This is happening even without any mask but the pattern is formed by metal structure that divides 4 inch wafer into several smaller regions.) > > Can anybody figure out what is my mistake? > > Thank you > Dimitar Dimitrov > _______________________________________________ > Hosted by the MEMS and Nanotechnology Exchange, the country's leading > provider of MEMS and Nanotechnology design and fabrication services. > Visit us at http://www.mems-exchange.org > > Want to advertise to this community? See http://www.memsnet.org > > To unsubscribe: > http://mail.mems-exchange.org/mailman/listinfo/mems-talk _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk