Hello, if a poor adhesion is the problem, I would suggest to use a metallic adhesion layer like chromium or titanium. Regards, André -----Ursprüngliche Nachricht----- Von: mems-talk-bounces+aboedecker=imsas.uni-bremen.de@memsnet.org [mailto:mems-talk-bounces+aboedecker=imsas.uni-bremen.de@memsnet.org] Im Auftrag von bhargav panchal Gesendet: Sonntag, 29. November 2015 18:01 An: General MEMS Discussion Betreff: [mems-talk] Silicon Carbide Issue We have problem regarding nickle deposition on Silicon nitride by sputtering. Prior to deposition we have removed the oxides from the surface. Please suggest possible solution. Have a good day everyone. Regards, Bhargav Panchal+91 9742712671 _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk