 Tell 'em Shay.
Keep in mind, I beleive all current formulations of photodefinable BCB and PI
are negative acting.  You also have to purchase the accompanying developer.
Neal Ricks
Haleos, Inc.
  shay kaplan  wrote: try phosensitive polyimide or BCB
Shay Kaplan

"Martin O. Patton" wrote:

> Dear mems-talkers,
>
> Is there a photoimageable insulator that can be applied to insulate trenches
> in III-V wafers from metal contacts which cross the trenches? I only have
> wet chemistry, so don't tell me to RIE.
>
> Thanks,
>
> Marty
>
> Martin O. Patton
> Senior Research Engineer
> Essential Research Inc.
> 6410 Eastland Road Suite D
> Cleveland, Ohio 44142
> www.er.com
> _______________________________________________
> mems-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
_______________________________________________
mems-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/
Yahoo! Health - your guide to health and wellness

reply