Dear lu Here is the etchant of titanium. Photoresist can be used by masking layer HF + HNO3 + H2O (1 : 1 : 50 ) Choe, S-H Esashi Lab. Tohoku University E-Mail: choe@mems.mech.tohoku.ac.jp