Dear all, Since we don't have equipment for anodic bonding in the lab, I need to figure out how to bond silicon and glass together by fusion bonding? However, I tried lots of pieces and they all failed. I did HF and RCA 1 clean for both silicon substrate (with pattern on it) and glass before bonding but it 's not bonding. Does anyone have done silicon and glass fusion bonding before? Any suggestions will be appreciated. Thank you. Best, Jingru