PDMS fine structures
DEBASHIS MAJI
2010-12-14
Dear All,

Thanks for your comments and suggestions. Actually I dont have either silane
or the teflon coating with me. I'll try to get them and see. Meanwhile I
shall try to reduce the baking temp of PDMS and check out...

Do you all suggest to clean up the Su8 master after each moulding process
with some chemicals or ultrasonication?

Please advise.
Thanks in advance.

Debashis Maji