Hi Yusuf, I contacted the person, in imec for the solvent, he actually used it for dissolving uncured PDMS, I my case it is cured. So I think the latest idea is to purchase dynasolve 210 for dissolving this cures PDMS. But we will also try it with the solvent used for dissolving uncured PDMS as well. I shall update with the results. Cheers, Righeira