Dear community, I have read information about the liftoff of ALD insulator ( http://marcuslab.harvard.edu/papers/Biercuk_ALD_APL.pdf). In the paper they have also reported the electrical measurement of a triple layer capacitor consisting of Pt-insulator-Pt. My question is, what can be the easiest way to electrically access the bottom contact layer right under the ALD wrap? Thanks a lot and welcome any comments if you happen to know more details about the measurement done in that paper. Best, Josh