Hi all, that's correct. You can call PDMS also silicone (not silicon!). Regards, André -----Ursprüngliche Nachricht----- Von: mems-talk-bounces+aboedecker=imsas.uni-bremen.de@memsnet.org [mailto:mems-talk-bounces+aboedecker=imsas.uni-bremen.de@memsnet.org] Im Auftrag von DEBASHIS MAJI Gesendet: Donnerstag, 9. Januar 2014 18:38 An: General MEMS discussion Betreff: Re: [mems-talk] Bio-compatible epoxy Dear Jan, PDMS stands for Polydimethlysloxane. It is a polymer often used for making biomedical devices. I need the epoxy to fix my device (made of PDMS) over some PE (polyethylene) or PU (polyurethane) substrates. Thanks for your help anyways. On Thu, Jan 9, 2014 at 2:43 AM, Jan Thorenwrote: > Our binder is very fast drying- like 5-10 minutes- I have a background in > architecture and do not know what PDMS is -- > so please describe it or let me know what the letters stand for. thanks- > Jan > > > > > Recreating Architecture through Nanotechnology > > > JanThoren-president > NanoArchitech > Architectural Technology Group > San Francisco Bay Area > > 707 741-7919 direct line > > nanoarchitech.com > > > > > > > > On Wed, Jan 8, 2014 at 8:52 AM, DEBASHIS MAJI >wrote: > > > Thanks all for your help... I shall try out the links and search for the > > epoxy. > > I tried fixing with PDMS, but my substrate itself is PDMS and it takes > some > > time to cure. so i am looking for an adhesive that binds quicker. > > I shall try out the links and search for the epoxy. > > > > > > > > On Wed, Jan 8, 2014 at 10:01 PM, DEBASHIS MAJI > >wrote: > > > > > Thanks Jan, > > > My material is PDMS. I would like to fix it on some PE or PU > substrates. > > > Would it be suitable for fixing of PDMS materials? > > > > > > > > > On Tue, Jan 7, 2014 at 8:50 PM, Jan Thoren wrote: > > > > > >> I have a material which is friendly to the human body and has very > good > > >> bonding abilities . It is non - conductive. > > >> What is the substrate material? > > >> I would be willing to test it if you can provide a sample of the > > material. > > >> My email is enoneves@gmail.com > > >> > > >> > > >> > > >> > > >> Recreating Architecture through Nanotechnology > > >> > > >> > > >> JanThoren-president > > >> NanoArchitech > > >> Architectural Technology Group > > >> San Francisco Bay Area > > >> > > >> 707 741-7919 direct line > > >> > > >> nanoarchitech.com > > >> > > >> > > >> > > >> > > >> > > >> > > >> > > >> On Sun, Jan 5, 2014 at 10:27 PM, DEBASHIS MAJI < > ece.debashis@gmail.com > > >> >wrote: > > >> > > >> > Dear All, > > >> > > > >> > I am searching for a some biocompatible epoxy (not conductive epoxy) > > to > > >> fix > > >> > my sensor over a substrate for some in vitro animal experiments. can > > >> > anybody kindly provide me names of few such epoxies? > > >> > > > >> > Thanks in advance. > > >> > > > >> > -- > > >> > Thanks & Regards > > >> > > > >> > Debashis Maji, > > >> > Senior Research Fellow, > > >> > PhD Scholar - School of Medical Science & Technology, > > >> > IIT Kharagpur, India - 721302 > > >> > _______________________________________________ > > >> > Hosted by the MEMS and Nanotechnology Exchange, the country's > leading > > >> > provider of MEMS and Nanotechnology design and fabrication services. > > >> > Visit us at http://www.mems-exchange.org > > >> > > > >> > Want to advertise to this community? See http://www.memsnet.org > > >> > > > >> > To unsubscribe: > > >> > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > > >> > > > >> _______________________________________________ > > >> Hosted by the MEMS and Nanotechnology Exchange, the country's leading > > >> provider of MEMS and Nanotechnology design and fabrication services. > > >> Visit us at http://www.mems-exchange.org > > >> > > >> Want to advertise to this community? See http://www.memsnet.org > > >> > > >> To unsubscribe: > > >> http://mail.mems-exchange.org/mailman/listinfo/mems-talk > > >> > > > > > > > > > > > > -- > > > Thanks & Regards > > > > > > Debashis Maji, > > > Senior Research Fellow, > > > PhD Scholar - School of Medical Science & Technology, > > > IIT Kharagpur, India - 721302 > > > > > > > > > > > -- > > Thanks & Regards > > > > Debashis Maji, > > Senior Research Fellow, > > PhD Scholar - School of Medical Science & Technology, > > IIT Kharagpur, India - 721302 > > _______________________________________________ > > Hosted by the MEMS and Nanotechnology Exchange, the country's leading > > provider of MEMS and Nanotechnology design and fabrication services. > > Visit us at http://www.mems-exchange.org > > > > Want to advertise to this community? See http://www.memsnet.org > > > > To unsubscribe: > > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > > > _______________________________________________ > Hosted by the MEMS and Nanotechnology Exchange, the country's leading > provider of MEMS and Nanotechnology design and fabrication services. > Visit us at http://www.mems-exchange.org > > Want to advertise to this community? See http://www.memsnet.org > > To unsubscribe: > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > -- Thanks & Regards Debashis Maji, Senior Research Fellow, PhD Scholar - School of Medical Science & Technology, IIT Kharagpur, India - 721302 _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk