Kirt Williams
2018-03-23
KI (potassium iodide) + I2 (iodine) also etches gold, but not silver, and
doesn't attack photoresist (but the PR sometimes peels).
I measured an etch rate for evaporated gold of 660 nm/min for a commercial mix
called AU-5 from Cyantek.

     Kirt Williams
     kirt_williams@ieee.org   cell 650-224-3503

-----Original Message-----
From: Bob Henderson [mailto:bob.henderson@etchedintimeinc.com]
Sent: Saturday, March 17, 2018 10:14 AM
To: 'General MEMS discussion'
Subject: Re: [mems-talk] Potassium iodate effect on gold?

Mario:

We used to call that mixture "Turkey Blood" and it does a fine job etching gold
and silver and still preserving the photo resist pattern you might remove if you
used something like Aqua Regia. Bob Henderson


-----Original Message-----
From: Gianmario Scotti [mailto:gianmario.scotti@gmail.com]
Sent: Thursday, March 15, 2018 3:32 AM
To: General MEMS discussion
Subject: [mems-talk] Potassium iodate effect on gold?

Hello all,


I have what might sound as an odd question, but hear me out nonetheless:
what effect does potassium iodate have on pure gold (let's say, evaporated)? Or
does the gold perhaps reduce the iodate?


Thanks in advance,


mario


--
Gianmario Scotti

Researcher
Leibniz-Institut für Ostseeforschung Warnemünde Seestraße 15
18119 Rostock
Germany

Visiting researcher
Aalto University, School of Electrical Engineering http://elec.aalto.fi/en/


Micronova, Tietotie 3
02150 Espoo
Finland
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply