Gold film
Gurvinderjit Singh
2002-05-20
Dear friend i have one query.
I am depositing gold film (thickness 0.1 micron)by thermal evaporation on
oxides,
but when  i am annealing my sample to 700K this gold film become non
-conductive may be  duo to formation of gold oxide. But from
literature i found
that gold should not become oxide till 1200K. I also read people using
gold electrodes (thin film by thermal evaporation) on their samples and
work till 900k kindly let me know where i am doing mistake, wether to take
more thick film or something else.



_______________________________________________________________________________


   Gurvinderjit Singh Ahluwalia             Tel: +91-0731-488656
     Laser Materials Division               Fax: +91-0731-488650
   Centre for Advanced Technology         email: gjit@cat.ernet.in
   Indore - 452 013  INDIA

_______________________________________________________________________________

reply