> Hi, We are looking for supplier who can drill more than 1 mm holes on
thick
> (1 mm) Pyrex glass wafers. Please write to propak@singnet.com.sg Regards.

Check with Sensor Prep Services in Illinois at 630-365-9645.
They do ultrasonic drilling through even thicker glass.