Making holes in Pyrex glass wafers?
2003-07-03
2003-07-02
2003-07-03
Making holes in Pyrex glass wafers?
Bill Flounders
2003-07-07
Alternate Ultrasonic Machining Contact:
Perhaps related?

J.A. Anderson Associates
Precision Glass/Ceramics and Ultrasonic Machining
630-377-6565
john@jaanderson.com
www.jaanderson.com

Bill Flounders, Ph.D.
Technology Manager
Berkeley Microlab




Kirt & Erika Zipf-Williams wrote:
>>Hi, We are looking for supplier who can drill more than 1 mm holes on
>
> thick
>
>>(1 mm) Pyrex glass wafers. Please write to propak@singnet.com.sg Regards.
>
>
> Check with Sensor Prep Services in Illinois at 630-365-9645.
> They do ultrasonic drilling through even thicker glass.
>
>     --Kirt Williams, Ph.D.   consultant
>
>
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/



reply