Hi,
I am using SU-8 2000 series and may need to use it on glass wafers.  Can anyone
suggest how I can make SU-8 adhere to glass, whether I need to spin coat
Omnicoat or treat the glass with oxygen plasma?
Also, how do I dice the glass wafers?  I have tried using a manual diamond
scriber but it does not cut the glass in straight lines.