durusmail: mems-talk: Glass-glass bonding problem
Glass-glass bonding problem
2011-08-16
2011-08-16
2011-08-17
2011-08-17
2011-08-17
2011-08-18
Glass-glass bonding problem
ashwini jambhalikar
2011-08-19
At what voltages/ temperatures, you have experimented?
I had bonded si-glass at 600 volts and 375 degree centigrade,
and when applied reverse potential at 1500 volts and 250 degree
centigrade(here i am attempting to bond above pair with a kovar
substrate), I found there is a formation of brown dots and a tendency
to debond.

ashwini

On Thu, Aug 18, 2011 at 7:56 PM, Shay  wrote:
> No debonding - the bond is permanent
>
> shay
reply