Xiaohui Lin
2011-11-09
I used MA6 aligner, 7.4mW, 8s exposure

On Wed, Nov 9, 2011 at 6:30 AM, Kuijpers, Peter
wrote:

> Hi all,
>
> What is the energy you've used?
>
> regards,
>
> Peter Kuijpers

--