try developing it for more time 30 seconds in developer another 30 seconds in fresh developer then IPA for 30 seconds also increase the dose alittle bit On Fri, Nov 11, 2011 at 1:11 AM, Xiaohui Linwrote: > could you advise what is adequate rinsing? I dip in SU8 developer for > 20-30s then rinse with IPA. Is it the correct step? > > I do notice the white stains if under-develop, for example, IPA rinse after > just 10s developing. > > > Thanks.