Hi Andrew,

I haven't used it yet. Can you brief me on how it works?

Thanks
Forum

-----Original Message-----
From: Andrew Sarangan [mailto:asarangan@gmail.com]
Sent: Thursday, July 09, 2009 4:57 PM
To: General MEMS discussion
Subject: Re: [mems-talk] Peel off PDMS

Have you tried using sigmacote (or jerseycote)?