Mario,
It should be ok. Might be something in the surface preparation or base
pressure and atmosphere in the system.

-----Original Message-----
From: mems-talk-bounces+shay=mizur.com@memsnet.org
[mailto:mems-talk-bounces+shay=mizur.com@memsnet.org] On Behalf Of Gianmario
Scotti
Sent: Thursday, June 25, 2015 1:21 PM
To: General MEMS discussion
Subject: [mems-talk] Improving adhesion of sputtered metals on borofloat
glass

Hey all,


I am sputtering platinum on borofloat (i.e. "pyrex") glass using ~10 nm of
chromium as adhesion layer. Adhesion seems poor, and I am looking at various
ways to improve it. Could you suggest some?



mario






--
Gianmario Scotti

Post-doc researcher
Helsinki University
Division of Pharmaceutical Chemistry and Technology Viikinkaari 5E (PO Box
56) FI-00014 http://www.helsinki.fi/pharmacy/chemtech/en/index.html


Visiting researcher
Aalto University, School of Electrical Engineering http://elec.aalto.fi/en/


Micronova, Tietotie 3
02150 Espoo
Finland
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk


_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply